Shape: Round, Flat, Square.
Size Range:
|
Diameter(mm) |
Thickness (mm) |
Width (mm) |
Length(mm) |
Round |
50-420 |
- |
- |
2000-5800 |
Square |
50-420 |
- |
- |
2000-5800 |
flat |
- |
20-50 |
80-600 |
2000-5800 |
Delivery condition:
Annealed, Quenched + Tempered
Surface state:
Black, Grinded, Peeled, Rough turned, Polished
Feature
1.Competitive price
2.immediate delivery
3.Premium quality
4.Reliable service
5.MOQ: 1 ton
Packing details |
In seaworthy packing, as your requirement. |
Delivery details |
within 30-50 days |
Chemical composition:
C |
Mn |
P |
S |
Si |
Cr |
V |
W |
Mo |
0.32-0.45 |
0.20-0.50 |
0.030max |
0.030max |
0.15-0.50 |
4.0-4.75 |
1.75-2.20 |
3.75-4.50 |
0.30-0.55 |
Heat treatment:
Hardness :Annealed(+A) max: 241 BHN
H19 tool steel when heat-treatment the preheat Temperature need reach 788°C, and the temperature may be ± 14 °C .
H19 tool steel when austenitizing ,should keep 5-15 minutes long. If is the salt bath ,temperature should keep in the 1177 °C , and shall be ± 5.6 °C. Or is the controlled atmosphere furnaces , temperature should keep in the 1191 °C , and shall be ± 5.6 °C.
Quenching: H19 tool steel Hardening quenching using air cooling, and it's hardness min is 55 RC.
Tempering: H19 tool steel general tempering temperature is 552°C. Double tempering of Double tempering of H19 tool steel is recommended.